P2000 / 1.4452

Chemical composition of Alloy P2000

C Mn Cr N
≤ 0.15 % 12.0-16.0 % 16.0-20.0 % 0.75-1.00
Mo Nb Fe Ni
% 2.5-4.2 ≤ 0.25 rest nickel free

Mechanical properties of Alloy P2000

solution heat treated typical values
tensile s Rm 980-1120 MPa
yield strength Rp 0,2 610-720 MPa
elongation after fracture 55-65 %
reduction of area A 65-75 %
cold worked precipitation hardened typical values
tensile strength Rm over 2000 MPa possible

Delivery program

dimensions (Ø) mm for samples only
0.8
1.02
1.30